- 1. Die must be processed when new (preferred prior to sampling*)
(*changes made after first sampling will be reprocessed
"no charge" or for minimal cost).
|
- 2. Die must have at least both sides (cover, ejector) processed.
|
- 3. Die must be re-processed at least at it's normal (≥ 40-60%) half
life or sooner.
|
- 4. Die must have expected shot life stated initially prior to
processing when new.
|
- 5. Die must not have pre-mature failure ( failure prior to half life
processing ).
|
- 6. If engineering changes are made after
MetaLLife
processing, guarantee is void
unless die is reprocessed.
|
Guarantee is limited to amount invoiced for
processing. Badger is not responsible for any consequential and/or
incidental costs or expenses incurred by customer. Guarantee is non-transferrable
from original invoiced agent or die casting company. |